Fe:SrTiO3
Iron-doped strontium titanate and strontium titanate single crystal have a similar structure. At present we can provide Fe:SrTiO3 single crystal substrates with iron doping concentration of: 0.05%, 0.04%.
Main Property Parameters | |
Crystal System | Cubic |
Growth Method | Flame |
Crystal Lattice Constant | a=3.905Å |
Doping Concentration(Fe%) | 0.005%,0.04% |
Melt Point(℃) | 2080 |
Density | 5.122(g/cm3) |
Hardness | 6-6.5(mohs) |
Dielectric Constant | ε=5.20 |
Chemical Stability | Insoluble in water |
Thermal Expansion | 10.4×10E-6/k |
Tangent Loss | ~5×10E-4(300k) ~3×10E-4(77k) |
Dimension(mm) | 5×5m、10×5m、10×10mm、15×15mm、20×20mm According to customer needs, substrates with special orientation and size can be customized. |
Thickness | 0.5mm、1.0mm |
Dimensional tolerance | <±0.1mm |
Thickness tolerance | <±0.05mm special requirements <±0.005mm) |
Polishing | One side or two sides |
Orientation tolerance | ±0.5° |
Flat Orientation tolerance | 2°(special requirements <1°) |
Orientation | <100>、<110>、<111> |
Packaging | Clean bag (100), Super clean room (1000) |