Nd:SrTiO3
Neodymium-doped strontium titanate has a similar structure to strontium titanate single crystal. At present, we can provide Nd:SrTiO3 single crystal substrates with Neodymium doping concentration of: 0.05%.
Main performance parameters | |
Crystal structure | Cube |
Crystal growth method | Verneuil |
Lattice constant | a=3.905Å |
Nd concentration (wt%) | 0.05% |
Melting point(℃) | 2080 |
Density(g/cm3) | 5.122(g/cm3) |
Hardness | 6-6.5(mohs) |
Coefficient of thermal expansion(/℃) | 9.4×10-6 |
Dielectric constant | ε=5.20 |
Chemical stability | Insoluble in water |
热膨胀系数 | 10.4×10E-6/k |
Secant loss | ~5×10E-4(300k) ~3×10E-4(77k) |
Size | 5×5m、10×5m、10×10mm、15×15mm、20×20mm Can be customized according to customer needs, special direction and size of the substrate. |
Thickness | 0.5mm、1.0mm |
Dimensional tolerance | <±0.1mm |
Thickness tolerance | <±0.05mm,Special requirements can be met<±0.005mm) |
Polishing | Single-sided or double-sided |
Crystal orientation | ±0.5° |
Flat orientation accuracy | 2°(Special requirements can reach within 1°) |
Crystal orientation | <100>、<110>、<111> etc. |
Package | Class 100 clean bag, Class 1000 super clean room |